It is currently not possible to order printed and bound versions of standards. This is due to challenges related to our printing supplier. We are working to resolve the situation and apologize for any inconvenience this may cause. For other options, contact salg@standard.no.
Standard

NEK EN 60317-48:2012

Published

Corrigenda and amendments are bought separately.

Language
Services

Abstract

IEC 60317-48:2012 specifies requirements of glass-fibre wound resin or varnish impregnated, bare, grade 1 or grade 2 enamelled round copper winding wire, temperature index 155. The impregnating agent can be, for instance, polyester or polyesterimide resin based. For this type of wire, the heat shock test is inappropriate and therefore a heat shock temperature cannot be established. Consequently, a class based on the requirements for temperature index and heat shock temperature cannot be specified. This edition includes the following significant technical changes with respect to the previous edition: - new subclause containing general notes on winding wire, - formerly part of the scope, - new subclause containing requirements for appearance, - new Clause 23, Pin hole test. Keywords: copper winding wire

Document information

  • Standard from NEK
  • Published:
  • Edition: 1
  • Version: 1
  • Document type: NAT
  • National Committee NEK/NK55

Product Relations