Abstract

Form This specification covers a silver alloy in the form of wire, rod, sheet, strip, foil, pig, powder, shot, and chips and a viscous mixture (paste) of powder in a suitable binder. Application This material has been used typically for joining ferrous metals, including austenitic steels and alloys, requiring moderate joint strength up to 700 °F (371 °C) for short-time service or up to 400 °F (204 °C) for long-time service, and for joining nonferrous metals except those having a base of aluminum, magnesium, or titanium, but usage is not limited to such applications. The nickel content helps minimize crevice corrosion in corrosion resistant steels.

Document information

  • Standard from SAE_AC
  • Published:
  • Version: 0
  • Document type: IS
  • Additional information
  • (Composition similar to UNS P07630)